Annealing |
Quenching |
Tempering |
Normalizing |
Q & T |
√ |
√ |
√ |
√ |
√ |
C ≤ |
Si ≤ |
Mn ≤ |
P ≤ |
S ≤ |
Cr | Ni |
---|---|---|---|---|---|---|
0.32-0.45 | 0.8-1.2 | 0.2-0.5 | 0.03 | 0.03 | 4.75-5.5 | |
Mo | Al | W | Nb | Ti | V | Ce |
1.1-1.75 | 0.8-1.2 | |||||
N | Co | Pb | B | Other | ||