Annealing |
Quenching |
Tempering |
Normalizing |
Q & T |
√ |
√ |
√ |
√ |
√ |
C |
Si ≤ |
Mn ≤ |
P ≤ |
S ≤ |
Cr | Ni | Mo | Other |
---|---|---|---|---|---|---|---|---|
≤0.030 | 1.00 | 2.00 | 0.035 | 0.015 | 21.0-23.0 | 4.50-6.50 | 2.50-3.50 | N 0.10-0.22 |