Annealing |
Quenching |
Tempering |
Normalizing |
Q & T |
√ |
√ |
√ |
√ |
√ |
C ≤ |
Si ≤ |
Mn ≤ |
P ≤ |
S ≤ |
Cr | Ni |
---|---|---|---|---|---|---|
0.03 | 0.6 | 0.7 | 0.03 | 0.02 | 19-22 | ... |
Mo | Al | Cu | Nb+Ta | Ti | V | Fe |
10-13 | ≤0.5 | ≤0.3 | ≤0.15 | 12-15 | ||
N | Co | Pb | W | Other | ||
≤1.0 | 1.0-2.0 | |||||
Click the Get Adobe Reader button to download the Adobe Reader:
Related steel grade search:AWS ENiCrMo-18
Previous pageUNS W86200