Annealing |
Quenching |
Tempering |
Normalizing |
Q & T |
√ |
√ |
√ |
√ |
√ |
C ≤ |
Si ≤ |
Mn ≤ |
P ≤ |
S ≤ |
Cr | Ni |
---|---|---|---|---|---|---|
0.08 | 1 | 2 | 0.045 | 0.03 | 17-19 | 9-13 |
Mo | Al | Cu | Nb | Ta | V | Ce |
≤0.1 | ||||||
N | Co | Pb | B | Other | ||
≤0.2 | Nb+Ta 10*C~1.0 | |||||
Click the Get Adobe Reader button to download the Adobe Reader:
Related steel grade search:S34800