Annealing |
Quenching |
Tempering |
Normalizing |
Q & T |
√ |
√ |
√ |
√ |
√ |
C ≤ |
Si ≤ |
Mn ≤ |
P ≤ |
S ≤ |
Cr | Ni |
---|---|---|---|---|---|---|
0.03-0.10 | 0.50 | 0.50 | 0.015 | 0.015 | 14.0-17.0 | /... |
Mo | Al | Cu | Nb | Ti | V | Ce |
≤0.50 | 1.10-1.35 | 2.00-2.60 | ||||
N | Co | Pb | B | Other | trade names | |
≤1.00 | Nb/T≤0.7~1.2 Fe5.00-9.00 | Inconel 751 | ||||
Click the Get Adobe Reader button to download the Adobe Reader:
Related steel grade search:N07031