Annealing |
Quenching |
Tempering |
Normalizing |
Q & T |
√ |
√ |
√ |
√ |
√ |
C ≤ |
Si ≤ |
Mn ≤ |
P ≤ |
S ≤ |
Cr | Ni |
---|---|---|---|---|---|---|
0.03 | 0.3-0.7 | 0.2-0.7 | 0.03 | 0.03 | 7.7-8.5 | |
Mo | Al | Cu | Nb | Ti | V | Ce |
0.3-0.5 | ||||||
N | Co | Pb | B | Other | ||