Home » Steel Grades > Alloy Steel > X1CrNiMoCuN 25-25-5

Category

Contact us

X1CrNiMoCuN 25-25-5

Data Table for: Steel Grades : Alloy Steel : X1CrNiMoCuN 25-25-5

Chemical composition(mass fraction)(wt.%)

Mechanical Properties

  • Quantity
  • Value
  • Unit
  • Young's modulus
  • Tensile strength
  • Elongation
  • Fatigue
  • Yield strength
  • 200000 - 200000
  • 650 - 880
  • 8 - 25
  • 275 - 275
  • 350 - 550
  • MPa
  • MPa
  • %
  • MPa
  • MPa

Physical Properties

  • Quantity
  • Value
  • Unit
  • Thermal expansion
  • Thermal conductivity
  • Specific heat
  • Melting temperature
  • Density
  • Resistivity
  • 10 - 10
  • 25 - 25
  • 460 - 460
  • 1450 - 1510
  • 7700 - 7700
  • 0.55 - 0.55
  • e-6/K
  • W/m.K
  • J/kg.K
  • °C
  • kg/m3
  • Ohm.mm2/m

Heat Treatment:

Annealing

Quenching

Tempering

Normalizing

Q & T

Can produce X1CrNiMoCuN 25-25-5 specifications and size

  • Steel grade
  • Specification
  • Processing range(mm)
  • X1CrNiMoCuN 25-25-5
  • X1CrNiMoCuN 25-25-5
  • X1CrNiMoCuN 25-25-5
  • X1CrNiMoCuN 25-25-5
  • X1CrNiMoCuN 25-25-5
  • X1CrNiMoCuN 25-25-5
  • Φ1 to Φ2000
  • 10 to 1000
  • 0.08 to 800(T)*10 to 1500(W)*Long
  • Pipe/tube/slugs/donuts/cubes/other shapes
  • OD: Φ4-410; WT: 1-35 mm
  • THK:0.1mm Width:1500mm

Description

 

Si 
Mn 
 P
 S
Cr   Ni  Mo  Other
  0.020  0.70  2.00  0.030  0.010  24.0-26.0  24.0-27.0  4.70-5.70  Cu 1.00-2.00
N 0.17-0.25

Standard download

More standard download >>

Click the Get Adobe Reader button to download the Adobe Reader:

Download Adobe Reader

Download Adobe Reader

Related steel grade search:X1CrNiMoCuN 25-25-5

Previous pageX2CrNiMoN 18-12-4
Next page:X2CrNiMoCuN 25-6-3