Annealing |
Quenching |
Tempering |
Normalizing |
Q & T |
√ |
√ |
√ |
√ |
√ |
C | Si | Mn | Ni | S | P | Cr | Mo | W | V | Ti | Cu |
0.09 - 0.16 | 0.17 - 0.37 | 0.4 - 0.7 | max 0.3 | max 0.025 | max 0.03 | 0.4 - 0.7 | 0.4 - 0.6 | max 0.2 | max 0.05 | max 0.03 | max 0.2 |